Fusion Frit FZ-556

Zinc matte frit for fast fire

Alternate Names: Fusion Frit FZ556

OxideAnalysisFormula
CaO15.00%0.444
K2O1.00%0.018
Na2O4.00%0.107
ZnO21.10%0.431
Al2O312.00%0.196
SiO247.60%1.316
Oxide Weight167.35
Formula Weight167.35
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.5 x 10-6
GSPT - Frit Softening Point 1800F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-556" descrip="Zinc matte frit for fast fire" searchkey="Fusion Frit FZ556" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="15.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="21.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved