Fusion Frit FZ-430

Calcium zinc frit

Alternate Names: Fusion Frit FZ430

OxideAnalysisFormula
CaO10.00%0.591
K2O2.00%0.070
Na2O4.00%0.214
ZnO1.50%0.061
SrO2.00%0.064
Al2O310.50%0.341
B2O311.50%0.548
SiO258.50%3.226
Oxide Weight331.42
Formula Weight331.42
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.45
GSPT - Frit Softening Point 1500F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-430" descrip="Calcium zinc frit" searchkey="Fusion Frit FZ430" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.500" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="2.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved