Fusion Frit FZ-390

Low zinc soft flux frit

Alternate Names: Fusion Frit FZ390

OxideAnalysisFormula
CaO2.00%0.200
Na2O8.20%0.742
ZnO0.85%0.059
Al2O35.50%0.302
B2O318.50%1.490
SiO265.00%6.064
Oxide Weight560.97
Formula Weight560.97
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 5.84 x 10-6
GSPT - Frit Softening Point 1450F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-390" descrip="Low zinc soft flux frit" searchkey="Fusion Frit FZ390" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.200" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.850" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="18.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="65.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved