Fusion Frit FZ-30

Zinc barium artware, tile, sanitaryware glaze frit

Alternate Names: Fusion Frit FZ30

OxideAnalysisFormula
BaO8.50%0.142
K2O4.00%0.109
Na2O1.40%0.058
ZnO16.00%0.505
SrO7.50%0.186
Al2O31.00%0.025
B2O311.50%0.424
SiO239.60%1.692
ZrO210.50%0.219
Oxide Weight256.78
Formula Weight256.78
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.47 x 10-6
GSPT - Frit Softening Point 1550F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-30" descrip="Zinc barium artware, tile, sanitaryware glaze frit" searchkey="Fusion Frit FZ30" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="8.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.400" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="16.000" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="7.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="39.600" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="10.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved