Fusion Frit FZ-276

Alternate Names: Frit FZ276

OxideAnalysisFormula
CaO5.85%0.491
K2O0.14%0.007
Na2O5.85%0.444
ZnO1.00%0.058
Al2O37.10%0.328
B2O312.00%0.812
SiO259.41%4.654
ZrO28.65%0.331
Oxide Weight470.80
Formula Weight470.80
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-276" descrip="" searchkey="Frit FZ276" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.850" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.140" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.850" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="59.410" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="8.650" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved