Fusion Frit FZ-24

High expansion leadless frit

Alternate Names: Frit FZ24

OxideAnalysisFormula
BaO1.40%0.022
CaO3.00%0.130
K2O8.00%0.206
Na2O14.70%0.576
ZnO2.20%0.066
Al2O310.00%0.238
B2O36.20%0.216
SiO254.50%2.203
Oxide Weight242.92
Formula Weight242.92
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 11.13 x 10-6
GSPT - Frit Softening Point 1450F

This is used as an addition to low and medium fire glazes to increase their thermal expansion to solve shivering problems.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-24" descrip="High expansion leadless frit" searchkey="Frit FZ24" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="1.400" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="8.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="14.700" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved