Fusion Frit FZ-22

Zinc barium calcium frit

Alternate Names: Frit FZ22

OxideAnalysisFormula
BaO4.10%0.051
CaO14.30%0.484
MgO0.60%0.028
K2O4.00%0.081
Na2O1.60%0.049
ZnO13.20%0.308
Al2O38.20%0.153
B2O34.50%0.123
SiO249.30%1.557
Oxide Weight189.39
Formula Weight189.39
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-22" descrip="Zinc barium calcium frit" searchkey="Frit FZ22" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="4.100" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.600" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="13.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved