Alternate Names: Fusion Frit FZ16

OxideAnalysisFormula
CaO4.20%0.180
Na2O9.40%0.364
ZnO15.50%0.457
B2O330.20%1.041
SiO240.70%1.624
Oxide Weight239.87
Formula Weight239.87
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.90
GSPT - Frit Softening Point 1450F

This analysis was confirmed with Fusion Dec 2017.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-16" descrip="Soft zinc flux for texture glazes" searchkey="Fusion Frit FZ16" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="9.400" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="15.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="30.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="40.700" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved