Fusion Frit FZ-10

Zircon alkaline boro silicate frit

Alternate Names: Frit FZ10

OxideAnalysisFormula
CaO1.10%0.071
K2O4.70%0.181
Na2O12.00%0.703
ZnO1.00%0.045
Al2O310.00%0.356
B2O313.20%0.689
SiO245.00%2.719
ZrO212.90%0.380
Oxide Weight362.83
Formula Weight362.83
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit FZ-10" descrip="Zircon alkaline boro silicate frit" searchkey="Frit FZ10" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.700" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="12.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved