Fusion Frit F-79

Low expansion flux for high alumina bodies

Alternate Names: Fusion Frit F79

OxideAnalysisFormula
CaO4.80%0.452
Li2O0.50%0.089
K2O1.20%0.067
Na2O4.00%0.341
SrO1.00%0.051
Al2O39.00%0.466
B2O326.50%2.012
SiO253.00%4.660
Oxide Weight528.41
Formula Weight528.41
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 5.72
GSPT - Frit Softening Point 1500F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-79" descrip="Low expansion flux for high alumina bodies" searchkey="Fusion Frit F79" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.800" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="0.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.000" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="1.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="26.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved