Fusion Frit F-77

BOND FRIT

Alternate Names: Frit F77

OxideAnalysisFormula
CaO18.00%0.608
MgO4.30%0.202
Na2O6.20%0.190
Al2O32.50%0.046
B2O345.00%1.226
SiO224.00%0.757
Oxide Weight189.55
Formula Weight189.55
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-77" descrip="BOND FRIT" searchkey="Frit F77" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="18.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="4.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="45.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="24.000" tolerance=""/> </oxides> </material>