Fusion Frit F-74

Alkaline boron flux

Alternate Names: Fusion Frit F74

OxideAnalysisFormula
K2O1.40%0.054
Na2O16.00%0.946
Al2O34.00%0.144
B2O324.00%1.263
SiO254.60%3.329
Oxide Weight366.40
Formula Weight366.40
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.91 x 10-6
GSPT - Frit Softening Point 1450F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-74" descrip="Alkaline boron flux" searchkey="Fusion Frit F74" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="16.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="24.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved