Fusion Frit F-71

Alkaline flux for grinding wheels

Alternate Names: Fusion Frit F71

OxideAnalysisFormula
CaO6.00%0.231
K2O2.50%0.057
Na2O20.40%0.711
Al2O36.80%0.144
B2O36.00%0.186
SiO258.30%2.097
Oxide Weight216.21
Formula Weight216.21
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 11.31 x 10-6
GSPT - Frit Softening Point 1400F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-71" descrip="Alkaline flux for grinding wheels" searchkey="Fusion Frit F71" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="20.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved