Fusion Frit F-65

High barium boron frit for cone 06-1 glazes

Alternate Names: Fusion Frit F65

OxideAnalysisFormula
BaO27.50%0.650
Na2O6.00%0.350
Al2O35.50%0.195
B2O313.00%0.676
SiO248.00%2.892
Oxide Weight362.11
Formula Weight362.11
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.85
GSPT - Frit Softening Point 1450F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-65" descrip="High barium boron frit for cone 06-1 glazes" searchkey="Fusion Frit F65" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="27.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved