Fusion Frit F-5

Strontium Barium flux

Alternate Names: Fusion Frit F5

OxideAnalysisFormula
BaO11.73%0.207
CaO10.22%0.492
K2O2.42%0.069
Na2O1.72%0.075
SrO6.04%0.157
Al2O35.14%0.136
B2O36.12%0.237
SiO256.62%2.543
Oxide Weight269.99
Formula Weight269.99
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.13 x 10-6
GSPT - Frit Softening Point 1800F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-5" descrip="Strontium Barium flux" searchkey="Fusion Frit F5" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="11.730" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.220" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.420" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.720" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="6.040" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.140" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.120" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.620" tolerance=""/> </oxides> </material>