Fusion Frit F-582

Lithium low fire clear frit

Alternate Names: Fusion Frit F582

OxideAnalysisFormula
CaO5.70%0.297
Li2O3.50%0.343
K2O2.50%0.078
Na2O6.00%0.283
Al2O37.20%0.206
B2O315.60%0.655
SiO259.50%2.892
Oxide Weight292.08
Formula Weight292.08
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.5 x 10-6
GSPT - Frit Softening Point 1400F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-582" descrip="Lithium low fire clear frit" searchkey="Fusion Frit F582" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.700" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="3.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="59.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved