Fusion Frit F-578

High barium zero boron frit

Alternate Names: Fusion Frit 578

OxideAnalysisFormula
BaO25.50%0.505
CaO5.60%0.303
K2O3.80%0.123
Na2O1.40%0.069
Al2O313.00%0.387
SiO250.70%2.563
Oxide Weight303.88
Formula Weight303.88
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.2 x 10-6
GSPT - Frit Softening Point 1800F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-578" descrip="High barium zero boron frit" searchkey="Fusion Frit 578" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="25.500" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.700" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved