Fusion Frit F-577

Calcium magnesium zirconium matt frit

Alternate Names: Fusion Frit F577

OxideAnalysisFormula
CaO15.50%0.451
MgO12.60%0.510
Na2O1.50%0.039
Al2O33.50%0.056
B2O36.40%0.150
SiO255.00%1.493
ZrO25.50%0.073
Oxide Weight163.09
Formula Weight163.09
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 5.8 x 10-6
GSPT - Frit Softening Point 1700F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-577" descrip="Calcium magnesium zirconium matt frit" searchkey="Fusion Frit F577" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="15.500" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="12.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="5.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved