Fusion Frit F-567

Alkali boron frit

Alternate Names: Fusion Frit F567

OxideAnalysisFormula
CaO0.24%0.016
K2O5.61%0.218
Na2O12.95%0.766
Al2O311.41%0.410
B2O324.01%1.265
SiO245.78%2.793
Oxide Weight366.70
Formula Weight366.70
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.14 x 10-6
GSPT - Frit Softening Point 1450F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-567" descrip="Alkali boron frit" searchkey="Fusion Frit F567" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.240" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.610" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.950" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.410" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="24.010" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.780" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved