Fusion Frit F-563

Barium zircon matte frit

OxideAnalysisFormula
BaO32.10%0.639
CaO4.40%0.239
K2O0.58%0.019
Na2O2.10%0.103
Al2O32.78%0.083
B2O31.34%0.059
SiO247.20%2.395
ZrO29.50%0.235
Oxide Weight305.01
Formula Weight305.01
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.8 x 10-6
GSPT - Frit Softening Point 1825F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-563" descrip="Barium zircon matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="32.100" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.580" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.780" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="1.340" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.200" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="9.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved