Fusion Frit F-562

Alkali boron frit

Alternate Names: Fusion Frit F562

OxideAnalysisFormula
CaO0.16%0.012
K2O3.60%0.160
Na2O12.26%0.828
Al2O317.05%0.700
B2O329.83%1.795
SiO237.09%2.584
Oxide Weight418.70
Formula Weight418.70
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.06 x 10-6
MLRG - Frit Melting Range (C) 1450F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-562" descrip="Alkali boron frit" searchkey="Fusion Frit F562" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.160" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.260" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.050" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="29.830" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="37.090" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved