Fusion Frit F-561

Barium-Zircon Matte frit

Alternate Names: Fusion Frit F561

OxideAnalysisFormula
BaO24.60%0.740
K2O5.30%0.260
Al2O35.00%0.226
B2O311.50%0.762
SiO246.00%3.531
ZrO27.60%0.285
Oxide Weight461.40
Formula Weight461.40
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.5 x 10-6
GSPT - Frit Softening Point 1800F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-561" descrip="Barium-Zircon Matte frit" searchkey="Fusion Frit F561" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="24.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="7.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved