Fusion Frit F-524

Strontium Barium clear frit

Alternate Names: Fusion Frit F524

OxideAnalysisFormula
BaO2.00%0.047
CaO7.30%0.468
K2O2.60%0.099
Na2O2.10%0.122
SrO7.60%0.264
Al2O39.50%0.335
B2O312.00%0.620
SiO256.90%3.406
Oxide Weight359.71
Formula Weight359.71
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 5.17 x 10-6
GSPT - Frit Softening Point 1800F

Low fire base glaze, add 10% kaolin, adjust with other frits

Add Frit FZ-24 to increase thermal expansion to deal with shivering, add frit F-15 (more color forgiving) or Frit F-69 to reduce thermal expansion to deal with crazing.

This is an approximate analysis provided Aug 2013 (the BaO is accurate).
This frit is used in the excellent MK3330 cone 6 crystal clear dinnerware glaze.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-524" descrip="Strontium Barium clear frit" searchkey="Fusion Frit F524" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.100" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="7.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved