Fusion Frit F-520B

Calcium borate dinnerware frit

Alternate Names: Fusion Frit F520B

OxideAnalysisFormula
CaO7.00%0.577
K2O6.50%0.319
Na2O1.40%0.104
Al2O37.50%0.340
B2O311.60%0.770
SiO266.00%5.076
Oxide Weight462.19
Formula Weight462.19
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.55
GSPT - Frit Softening Point 1700F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-520B" descrip="Calcium borate dinnerware frit" searchkey="Fusion Frit F520B" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="6.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved