Fusion Frit F-498

High magnesium flux

Alternate Names: Fusion Frit F498

OxideAnalysisFormula
CaO15.50%0.474
MgO10.00%0.426
Na2O3.60%0.100
Al2O310.50%0.177
B2O316.60%0.409
SiO243.80%1.251
Oxide Weight171.68
Formula Weight171.68
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.92 x 10-6
GSPT - Frit Softening Point 1500F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-498" descrip="High magnesium flux" searchkey="Fusion Frit F498" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="15.500" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="10.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved