Fusion Frit F-496

Clear Alkali Boron Frit

Alternate Names: Fusion Frit F-496, Frit F496

OxideAnalysisFormula
K2O1.60%0.154
Na2O5.80%0.846
Al2O31.60%0.142
B2O316.00%2.080
SiO275.00%11.290
Oxide Weight904.70
Formula Weight904.70
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 4.66
GSPT - Frit Softening Point 1650F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-496" descrip="Clear Alkali Boron Frit" searchkey="Fusion Frit F-496, Frit F496" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.800" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="75.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved