Fusion Frit F-495

Calcium borate dinnerware soft flux

Alternate Names: Fusion Frit F495

OxideAnalysisFormula
CaO13.50%0.743
K2O1.00%0.033
Na2O4.50%0.224
Al2O39.00%0.272
B2O314.50%0.643
SiO257.50%2.954
Oxide Weight308.80
Formula Weight308.80
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.01
GSPT - Frit Softening Point 1800F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-495" descrip="Calcium borate dinnerware soft flux" searchkey="Fusion Frit F495" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="13.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved