Oxide Analysis Formula
K2O 6.00% 0.10
Li2O 11.00% 0.59
Na2O 11.70% 0.30
B2O3 13.20% 0.31
Al2O3 6.30% 0.10
SiO2 51.80% 1.39
Oxide Weight 160.89
Formula Weight 160.89

Notes

This analysis was confirmed with Fusion Sept 2013. Excellent for replacing Spodumene in glazes (to eliminate its frothing and bubbling issues), this contains a higher percentage of lithia plus contributes other oxides that most glazes need.

Related Information

Links

Materials Frit
Materials Lithium Carbonate
Suppliers Fusion Ceramics Inc
Typecodes Frit

Data

Co-efficient of Linear Expansion14.13
Frit Softening Point1300F

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved