Fusion Frit F-490C

Strontium frit

OxideAnalysisFormula
CaO9.00%0.529
K2O3.50%0.123
Na2O2.00%0.106
SrO7.60%0.242
Al2O310.30%0.333
B2O312.40%0.588
SiO255.20%3.029
Oxide Weight329.82
Formula Weight329.82
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-490C" descrip="Strontium frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.000" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="7.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved