Fusion Frit F-413

High sodium, boron-free, high expansion frit

Alternate Names: Fusion Frit 413

OxideAnalysisFormula
MgO0.50%0.043
Na2O17.00%0.957
Al2O35.50%0.188
SiO276.50%4.441
Oxide Weight347.17
Formula Weight347.17
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.67 x 10e-6
GSPT - Frit Softening Point 1600F

Popular in crystalline glazes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-413" descrip="High sodium, boron-free, high expansion frit" searchkey="Fusion Frit 413" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="17.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="76.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved