Oxide Analysis Formula
CaO 18.00% 0.61
MgO 4.30% 0.20
Na2O 6.20% 0.19
B2O3 45.00% 1.23
Al2O3 2.50% 0.05
SiO2 24.00% 0.76
Oxide Weight 189.55
Formula Weight 189.55

Related Information

Links

Materials Pemco Frit P-2201
Materials Frit
Materials Fusion Frit F-77
Suppliers Fusion Ceramics Inc
Typecodes Frit
Typecodes Gerstley Borate Substitutes
Be careful, many of these materials are approximate substitutes (e.g. they have similar chemistry but much different physical properties). There is no exact substitute.

Data

Co-efficient of Linear Expansion6.39 x 10-6
Frit Melting Range (C)1400F

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved