Fusion Frit F-304

Alternate Names: Frit F304

OxideAnalysisFormula
CaO18.00%0.695
MgO1.90%0.102
Na2O5.80%0.203
Al2O312.00%0.255
B2O36.50%0.202
SiO256.00%2.019
Oxide Weight217.09
Formula Weight217.09
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-304" descrip="" searchkey="Frit F304" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="18.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.900" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.800" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.000" tolerance=""/> </oxides> </material>