Fusion Frit F-280

All fritted cone 06 glazes

Alternate Names: Fusion Frit F280 Fusion

OxideAnalysisFormula
CaO14.20%0.680
K2O0.60%0.017
Na2O7.00%0.303
Al2O38.50%0.224
B2O315.00%0.579
SiO254.80%2.449
Oxide Weight268.80
Formula Weight268.80
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.9 x 10-6
GSPT - Frit Softening Point 1550F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-280" descrip="All fritted cone 06 glazes" searchkey="Fusion Frit F280 Fusion" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved