Fusion Frit F-245

Alkali boron bonding frit

Alternate Names: Fusion Frit F245

OxideAnalysisFormula
CaO3.00%0.312
Na2O7.30%0.688
Al2O30.90%0.052
B2O336.40%3.055
SiO252.40%5.092
Oxide Weight584.05
Formula Weight584.05
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 4.61
GSPT - Frit Softening Point 1550F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-245" descrip="Alkali boron bonding frit" searchkey="Fusion Frit F245" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.900" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="36.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.400" tolerance=""/> </oxides> </material>