Fusion Frit F-237

Alternate Names: Frit F237

OxideAnalysisFormula
CaO6.30%0.293
K2O2.30%0.064
Na2O15.30%0.643
Al2O33.70%0.095
B2O32.60%0.097
SiO258.55%2.540
ZrO211.25%0.238
Oxide Weight260.76
Formula Weight260.76
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-237" descrip="" searchkey="Frit F237" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.550" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="11.250" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved