Fusion Frit F-19

Boro Calcium Dinnerware Frit

Alternate Names: Fusion Frit F19

OxideAnalysisFormula
CaO14.20%0.692
Na2O7.00%0.308
Al2O39.70%0.260
B2O314.60%0.573
SiO254.50%2.478
Oxide Weight273.21
Formula Weight273.21
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.90
GSPT - Frit Softening Point 1550F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-19" descrip="Boro Calcium Dinnerware Frit" searchkey="Fusion Frit F19" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved