Fusion Frit F-18

Dinnerware Strontium Frit

Alternate Names: F18 Fusion, Frit F18, Frit F 18

OxideAnalysisFormula
CaO11.80%0.593
K2O2.40%0.072
Na2O2.60%0.118
SrO8.00%0.218
Al2O36.80%0.188
B2O38.90%0.360
SiO259.50%2.789
Oxide Weight281.71
Formula Weight281.71
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.13
GSPT - Frit Softening Point 1750F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-18" descrip="Dinnerware Strontium Frit" searchkey="F18 Fusion, Frit F18, Frit F 18" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.800" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.600" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="8.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="8.900" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="59.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved