Fusion Frit F-134

Strontium frit base for cone 5-6 glazes

Alternate Names: Fusion Frit F134

OxideAnalysisFormula
CaO11.00%0.569
Li2O0.40%0.039
K2O1.20%0.037
Na2O4.90%0.229
SrO4.50%0.126
Al2O311.50%0.327
B2O36.00%0.250
SiO260.50%2.920
Oxide Weight290.10
Formula Weight290.10
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.07 x 10-6
GSPT - Frit Softening Point 1800F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-134" descrip="Strontium frit base for cone 5-6 glazes" searchkey="Fusion Frit F134" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.000" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="0.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.900" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="4.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="60.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved