Fusion Frit F-12

Artware Flux Calcium Frit

Alternate Names: F12 Fusion,Frit F12

OxideAnalysisFormula
CaO20.00%0.680
Na2O10.40%0.320
Al2O30.80%0.015
B2O323.80%0.652
SiO245.00%1.428
Oxide Weight190.75
Formula Weight190.75
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.18
GSPT - Frit Softening Point 1450F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit F-12" descrip="Artware Flux Calcium Frit" searchkey="F12 Fusion,Frit F12" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="20.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="23.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved