Fusion Frit 5325

Low melting high expansion sodium borosilicate frit

OxideAnalysisFormula
CaO2.44%0.140
K2O5.85%0.200
Na2O12.71%0.660
Al2O39.19%0.290
B2O314.49%0.670
SiO255.29%2.960
Oxide Weight321.73
Formula Weight321.73
If this formula is not unified correctly please contact us.

Useful for raku glazes


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit 5325" descrip="Low melting high expansion sodium borosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.441" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.856" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.719" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.194" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.495" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.295" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved