Fusion Frit 435

Boron free high sodium frit

Alternate Names: Fusion Frit 435

OxideAnalysisFormula
CaO2.80%0.128
MgO1.50%0.096
K2O2.60%0.071
Na2O17.00%0.705
SiO276.10%3.256
Oxide Weight257.12
Formula Weight257.12
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.9 x 10-6
GSPT - Frit Softening Point 1650F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit 435" descrip="Boron free high sodium frit" searchkey="Fusion Frit 435" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.800" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="17.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="76.100" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved