Fusion Frit 294

Calcium Magnesium flux

Alternate Names: Fusion Frit 294

OxideAnalysisFormula
CaO33.20%0.684
MgO11.00%0.316
Al2O37.20%0.082
SiO248.60%0.935
Oxide Weight115.64
Formula Weight115.64
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.39 x 10-6
GSPT - Frit Softening Point 1750F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fusion Frit 294" descrip="Calcium Magnesium flux" searchkey="Fusion Frit 294" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="33.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="11.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved