FT-YB Clay

Westerwald, Germany - Plastic Clay

OxideAnalysisFormula
CaO0.30%0.021
MgO0.30%0.030
K2O1.40%0.059
Na2O0.10%0.006
TiO22.50%0.125
Al2O325.60%1.000
SiO257.30%3.799
Fe2O32.80%0.070
C0.40
LOI9.70
Oxide Weight359.79
Formula Weight400.21
If this formula is not unified correctly please contact us.

Raw Color - YELLOW
Particle Size (e.s.d.)
125 microns - 0.2
63 microns - 1.4
20 microns - 92
2 microns - 79
.5 microns - 64
Modulus of Rupture at 110C
Mn/M2 - 6.7
lbf/in2 - 970
Water Absorption
1120C - 4.0
1220C - 0.50
Shrinkage Dry to Fired
1120C - 7.5
1220C - 6.0
Plastic Index - 950
PF NO. - 39.0


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="FT-YB Clay" descrip="Westerwald, Germany - Plastic Clay" searchkey="" loi="10.10" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="2.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="25.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.300" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.800" tolerance=""/> </oxides> <volatiles> <volatile symbol="C" name="Carbon" percent="0.400" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="9.700" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved