FT-V Clay

Westerwald, Germany - Plastic Clay

OxideAnalysisFormula
CaO0.20%0.016
MgO0.30%0.033
K2O2.60%0.123
Na2O0.20%0.014
TiO21.30%0.073
Al2O322.80%1.000
SiO263.70%4.742
Fe2O32.30%0.064
C0.10
LOI6.60
Oxide Weight417.84
Formula Weight447.85
If this formula is not unified correctly please contact us.

Raw Color - CREAM
Particle Size (e.s.d.)
125 microns - 1.0
63 microns - 2.5
20 microns - 94
2 microns - 69
.5 microns - 47
Modulus of Rupture at 110C
Mn/M2 - 5.2
lbf/in2 - 750
Water Absorption
1120C - 3.5
1220C - 0.00
Shrinkage Dry to Fired
1120C - 9.0
1220C - 10.5
Refractoriness
Cone - 29, 1650C
Plastic Index - 923
PF NO. - 34.2


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="FT-V Clay" descrip="Westerwald, Germany - Plastic Clay" searchkey="" loi="6.70" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="22.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.300" tolerance=""/> </oxides> <volatiles> <volatile symbol="C" name="Carbon" percent="0.100" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="6.600" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved