FT-M Clay

Westerwald, Germany - Plastic Clay

OxideAnalysisFormula
CaO0.20%0.018
MgO0.30%0.037
K2O1.80%0.096
Na2O0.10%0.008
TiO21.70%0.106
Al2O320.40%1.000
SiO262.90%5.233
Fe2O34.60%0.144
C0.10
LOI7.00
Oxide Weight460.00
Formula Weight495.16
If this formula is not unified correctly please contact us.

Raw Color - LIGHT RED - DARK RED
Particle Size (e.s.d.)
125 microns - 1.8
63 microns - 6.1
20 microns - 85
2 microns - 58
.5 microns - 32
Modulus of Rupture at 110C
Mn/M2 - 6.2
lbf/in2 - 900
Water Absorption
1120C - 8.0
1220C - 2.00
Shrinkage Dry to Fired
1120C - 5.0
1220C - 7.5
Plastic Index - 643
PF NO. - 31.2


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="FT-M Clay" descrip="Westerwald, Germany - Plastic Clay" searchkey="" loi="7.10" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="20.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.900" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="4.600" tolerance=""/> </oxides> <volatiles> <volatile symbol="C" name="Carbon" percent="0.100" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="7.000" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved