FT-J Clay

Westerwald, Germany - Plastic Clay

OxideAnalysisFormula
CaO0.20%0.017
MgO0.20%0.024
K2O2.00%0.102
Na2O0.30%0.023
TiO21.30%0.078
Al2O321.30%1.000
SiO266.70%5.315
Fe2O31.80%0.054
C0.10
LOI6.30
Oxide Weight449.18
Formula Weight479.90
If this formula is not unified correctly please contact us.

Raw Color - CREAM
Particle Size (e.s.d.)
125 microns - 0.8
63 microns - 3.6
20 microns - 92
2 microns - 67
.5 microns - 52
Modulus of Rupture at 110C
Mn/M2 - 4.7
lbf/in2 - 680
Water Absorption
1120C - 8.0
1220C - 1.00
Shrinkage Dry to Fired
1120C - 7.0
1220C - 8.5
Refractoriness
Cone - 29, 1650C
Plastic Index - 616
PF NO. - 29.0


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="FT-J Clay" descrip="Westerwald, Germany - Plastic Clay" searchkey="" loi="6.40" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.300" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="21.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.800" tolerance=""/> </oxides> <volatiles> <volatile symbol="C" name="Carbon" percent="0.100" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="6.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved