FT-A Clay

Westerwald, Germany - Plastic Clay

OxideAnalysisFormula
CaO0.20%0.015
MgO0.10%0.010
K2O2.20%0.096
Na2O0.20%0.013
TiO21.40%0.072
Al2O324.90%1.000
SiO262.70%4.274
Fe2O31.00%0.026
C0.20
LOI7.30
Oxide Weight379.73
Formula Weight410.52
If this formula is not unified correctly please contact us.

Raw Color - WHITE-LIGHT GREY
Particle Size (e.s.d.)
125 microns - 0.4
63 microns - 1.7
20 microns - 92
2 microns - 69
.5 microns - 49
Modulus of Rupture at 110C
Mn/M2 - 6.4
lbf/in2 - 920
Water Absorption
1120C - 3.0
1220C - 0
Shrinkage Dry to Fired
1120C - 8.5
1220C - 11.0
Refractoriness
Cone - 31, 1690C
Plastic Index - 858
PF NO. - 33.6


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="FT-A Clay" descrip="Westerwald, Germany - Plastic Clay" searchkey="" loi="7.50" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="24.900" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.000" tolerance=""/> </oxides> <volatiles> <volatile symbol="C" name="Carbon" percent="0.200" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="7.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved