FT-201 Clay

Westerwald, Germany - Plastic Clay

OxideAnalysisFormula
CaO0.20%0.026
MgO0.30%0.055
K2O1.50%0.117
Na2O0.20%0.024
TiO21.30%0.119
Al2O313.90%1.000
SiO276.60%9.353
Fe2O32.10%0.096
C0.30
LOI4.00
Oxide Weight705.19
Formula Weight736.88
If this formula is not unified correctly please contact us.

Raw Color - CREAM
Particle Size (e.s.d.)
125 microns - 0.5
63 microns - 8.0
20 microns - 82
2 microns - 47
.5 microns - 35
Modulus of Rupture at 110C
Mn/M2 - 3.6
lbf/in2 - 530
Water Absorption
1120C - 0.5
1220C - 2.00
Shrinkage Dry to Fired
1120C - 2.0
1220C - 4.3
Refractoriness
Cone - 28, 1630C
Plastic Index - 500
PF NO. - 24.0


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="FT-201 Clay" descrip="Westerwald, Germany - Plastic Clay" searchkey="" loi="4.30" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.900" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="76.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="C" name="Carbon" percent="0.300" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="4.000" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved