FT-200 Clay

Westerwald, Germany - Plastic Clay

OxideAnalysisFormula
CaO0.10%0.019
MgO0.20%0.054
K2O1.00%0.115
Na2O0.10%0.018
TiO20.90%0.122
Al2O39.40%1.000
SiO285.20%15.383
Fe2O30.50%0.034
C0.10
LOI2.70
Oxide Weight1056.89
Formula Weight1087.34
If this formula is not unified correctly please contact us.

Raw Color - WHITE-LIGHT GREY
Particle Size (e.s.d.)
125 microns - 8.4
63 microns - 15.0
20 microns - 83
2 microns - 30
.5 microns - 16
Modulus of Rupture at 110C
Mn/M2 - 1.7
lbf/in2 - 240
Shrinkage Dry to Fired
1120C - 1.6
1220C - 4.2
Refractoriness
Cone - 28, 1630C
Plastic Index - 420
PF NO. - 20.0


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="FT-200 Clay" descrip="Westerwald, Germany - Plastic Clay" searchkey="" loi="2.80" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="85.200" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.500" tolerance=""/> </oxides> <volatiles> <volatile symbol="C" name="Carbon" percent="0.100" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="2.700" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved