Fritte M3

OxideAnalysisFormula
CaO0.36%0.419
MgO0.00%0.003
K2O0.21%0.146
Na2O0.41%0.432
Al2O30.20%0.129
SiO21.88%2.013
Oxide Weight198.31
Formula Weight198.31
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 855C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fritte M3" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.366" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.002" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.214" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.417" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.205" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="1.884" tolerance=""/> </oxides> </material>